JSR Butyl Rubber - IIR / CIIR / BIIR

Excels in Air Impermeability, Weather Resistance, Ozone Resistance, Heat Resistance, and Aging Resistance. The heat aging resistance is improved for chlorobutyl and bromobutyl in comparison with regular butyl rubbe

Grade Product Stain Unsaturation (mol %) Halogen Content (%) Mooney Viscosit ML1+4 (125 ℃ CBe) Specific Gravity Characteristics Application
JSR BUTYL 065 NS 0.8 - 32 0.92 Weather, Ozone, Chemical Resistance. Electric wire, cable, adhesive, construction materials, sealing materials
JSR BUTYL 268 NS 1.5 - 51 0.92 Low air impermeability, good heat resist. Inner tube, bladder, adhesive
JSR BUTYL 365 NS 2.0 - 33 0.92 Excels in heat & Chemical Resistance. Automotive parts, bladder, heat resistance hose, lining
JSR CHLOROBUTYL 1066 NS - Cl 1.2 38 0.92 Chlorobutyl Rubber Inner tube, inner liner,automotive parts,electric wire, industrial goods
JSR BUROMOBUTYL 2222 NS - Br 2 32 0.93 Bromobutyl Rubber
JSR BUROMOBUTYL 2244 NS - Br 2 46 0.93
JSR BUROMOBUTYL 2255 NS - Br 2 46 0.93